Wood Record

Brazilian rosewood vs Leche Perra

Dalbergia nigra against Helicostylis tomentosa. Every number below names the publication it came from.

PropertyBrazilian rosewoodLeche Perra
Janka hardness2,720 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-955.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture19,000 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b22,800 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.88 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.86 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength9,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)8.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-414.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.59USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.70Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Leche Perra carries 20% more load in bending, which matters for a shelf or a rail.
  • Brazilian rosewood is the heavier of the two by 146 kg/m³, which a reader building a door or a case should weigh.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons