PropertyBrazilian rosewoodMaçarandubarana
Janka hardness2,720 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,725 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-961.8 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture19,000 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b25,232 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.88 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b10,810 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)8.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-420.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.59USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.69LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Maçarandubarana carries 33% more load in bending, which matters for a shelf or a rail.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.