Wood Record

Breu-manga vs Muhuhu

Tetragastris altissima against Brachylaena hutchinsii. Every number below names the publication it came from.

PropertyBreu-mangaMuhuhu
Janka hardness2,169 lbfLPF/SFB Madeiras Brasileiras2,190 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC58.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture19,529 lb/in²LPF/SFB Madeiras Brasileiras16,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.08 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.46 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength11,079 lb/in²LPF/SFB Madeiras Brasileiras10,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)13.0%LPF/SFB Madeiras Brasileiras—
Tangential / radial ratio(lower is better)1.96LPF/SFB Madeiras Brasileiras—

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Breu-manga carries 21% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.