Wood Record

Breu vs Matamatá / sapucaia-amargosa

Protium sp. against Lecythis idatimon. Every number below names the publication it came from.

PropertyBreuMatamatá / sapucaia-amargosa
Janka hardness2,317 lbfLPF/SFB Madeiras Brasileiras2,341 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC39.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)60.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,012 lb/in²LPF/SFB Madeiras Brasileiras20,453 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.25 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.13 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,449 lb/in²LPF/SFB Madeiras Brasileiras10,055 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.0%LPF/SFB Madeiras Brasileiras15.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.92LPF/SFB Madeiras Brasileiras2.10LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Matamatá / sapucaia-amargosa is the heavier of the two by 343 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons