Wood Record

Bubinga vs East African Olive

Guibourtia spp. against Olea hochstetteri. Every number below names the publication it came from.

PropertyBubingaEast African Olive
Janka hardness2,690 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,740 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC55.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-955.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture22,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b25,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.48 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.53 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength10,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b12,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)14.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—
Tangential / radial ratio(lower is better)1.45USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—

What the numbers mean

  • The two match on hardness, within 2%. Choose on movement or on appearance instead.
  • East African Olive carries 12% more load in bending, which matters for a shelf or a rail.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.