Bubinga vs Mecrusse
Guibourtia spp. against Androstachys johnsonii. Every number below names the publication it came from.
| Property | Bubinga | Mecrusse |
|---|---|---|
| Janka hardness | 2,690 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2,540 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 55.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 22,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 18,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.48 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | — |
| Crushing strength | 10,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 9,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 14.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 11.6%Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Tangential / radial ratio(lower is better) | 1.45USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 1.07Chudnoff 1984, Tropical Timbers of the World (AH-607) |
What the numbers mean
- Bubinga resists denting better. It tests 6% harder than Mecrusse.
- Mecrusse moves more evenly. Its tangential-to-radial ratio is 1.1 against 1.4, so it is the safer choice for a wide flat panel.
- Bubinga carries 21% more load in bending, which matters for a shelf or a rail.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.