Bubinga vs Missanda
Guibourtia spp. against Erythrophleum ivorense. Every number below names the publication it came from.
| Property | Bubinga | Missanda |
|---|---|---|
| Janka hardness | 2,690 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2,930 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 55.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 22,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 23,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.48 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2.24 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 10,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 14,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 14.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | — |
| Tangential / radial ratio(lower is better) | 1.45USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | — |
What the numbers mean
- Missanda resists denting better. It tests 9% harder than Bubinga.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.