Wood Record

Bubinga vs Muhimbi

Guibourtia spp. against Cynometra alexandri. Every number below names the publication it came from.

PropertyBubingaMuhimbi
Janka hardness2,690 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,975 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC55.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-954.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture22,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b21,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.48 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.05 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength10,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b10,400 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)14.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—
Tangential / radial ratio(lower is better)1.45USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4—

What the numbers mean

  • Muhimbi resists denting better. It tests 11% harder than Bubinga.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons