Wood Record

Bulletwood vs Macawood

Manilkara bidentata against Platymiscium spp.. Every number below names the publication it came from.

PropertyBulletwoodMacawood
Janka hardness3,190 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b3,150 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)64.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture27,300 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b27,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity3.45 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b3.20 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength11,640 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b16,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)16.9%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-46.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.49USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.30USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons