Burma Lancewood vs Chengal

Homalium spp. against Balanocarpus spp.. Every number below names the publication it came from.

PropertyBurma LancewoodChengal
Janka hardness2,270 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,130 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture15,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)21,560 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.26 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.84 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength6,030 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)10,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)——

What the numbers mean

  • Burma Lancewood resists denting better. It tests 7% harder than Chengal.
  • Chengal carries 42% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.