Burma Lancewood vs Tembusu
Homalium spp. against Fagraea spp.. Every number below names the publication it came from.
| Property | Burma Lancewood | Tembusu |
|---|---|---|
| Janka hardness | 2,270 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,120 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 15,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 21,400 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.26 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 3.02 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 6,030 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 12,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | — | — |
| Tangential / radial ratio(lower is better) | — | — |
What the numbers mean
- Burma Lancewood resists denting better. It tests 7% harder than Tembusu.
- Tembusu carries 41% more load in bending, which matters for a shelf or a rail.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.