Wood Record

Burma Padauk vs Muhuhu

Pterocarpus macrocarpus against Brachylaena hutchinsii. Every number below names the publication it came from.

PropertyBurma PadaukMuhuhu
Janka hardness2,170 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,190 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC54.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture20,640 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)16,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.08 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.46 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength10,945 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)10,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)8.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Tangential / radial ratio(lower is better)1.71Chudnoff 1984, Tropical Timbers of the World (AH-607)—

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Burma Padauk carries 27% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons