Wood Record

Cachaporra-do-gentio vs Ipê

Terminalia cf argentea against Handroanthus serratifolius = Tabebuia serratifolia. Every number below names the publication it came from.

PropertyCachaporra-do-gentioIpê
Janka hardness3,139 lbfLPF/SFB Madeiras Brasileiras3,100 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC60.6 lb/ft³LPF/SFB Madeiras Brasileiras72.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,595 lb/in²LPF/SFB Madeiras Brasileiras24,549 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.86 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength12,275 lb/in²LPF/SFB Madeiras Brasileiras12,360 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.2%LPF/SFB Madeiras Brasileiras10.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.69LPF/SFB Madeiras Brasileiras1.34LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Ipê moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.7, so it is the safer choice for a wide flat panel.
  • Ipê carries 19% more load in bending, which matters for a shelf or a rail.
  • Ipê is the heavier of the two by 191 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons