Cachaporra-do-gentio vs Macawood
Terminalia cf argentea against Platymiscium spp.. Every number below names the publication it came from.
| Property | Cachaporra-do-gentio | Macawood |
|---|---|---|
| Janka hardness | 3,139 lbfLPF/SFB Madeiras Brasileiras | 3,150 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Density at 12% MC | 60.6 lb/ft³LPF/SFB Madeiras Brasileiras | 64.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 20,595 lb/in²LPF/SFB Madeiras Brasileiras | 27,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Modulus of elasticity | 2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 3.20 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Crushing strength | 12,275 lb/in²LPF/SFB Madeiras Brasileiras | 16,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Volumetric shrinkage(lower is better) | 15.2%LPF/SFB Madeiras Brasileiras | 6.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 |
| Tangential / radial ratio(lower is better) | 1.69LPF/SFB Madeiras Brasileiras | 1.30USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Macawood moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.7, so it is the safer choice for a wide flat panel.
- Macawood carries 34% more load in bending, which matters for a shelf or a rail.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.