Cachaporra-do-gentio vs Macucu-branco
Terminalia cf argentea against Licania oblongifolia. Every number below names the publication it came from.
| Property | Cachaporra-do-gentio | Macucu-branco |
|---|---|---|
| Janka hardness | 3,139 lbfLPF/SFB Madeiras Brasileiras | 3,153 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 60.6 lb/ft³LPF/SFB Madeiras Brasileiras | 58.7 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 20,595 lb/in²LPF/SFB Madeiras Brasileiras | 19,429 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.19 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,275 lb/in²LPF/SFB Madeiras Brasileiras | 10,895 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.2%LPF/SFB Madeiras Brasileiras | 19.6%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.69LPF/SFB Madeiras Brasileiras | 1.97LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Cachaporra-do-gentio moves more evenly. Its tangential-to-radial ratio is 1.7 against 2.0, so it is the safer choice for a wide flat panel.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.