Cachaporra-do-gentio vs Pracuúba-da-terra-firme
Terminalia cf argentea against Trichilia lecointei. Every number below names the publication it came from.
| Property | Cachaporra-do-gentio | Pracuúba-da-terra-firme |
|---|---|---|
| Janka hardness | 3,139 lbfLPF/SFB Madeiras Brasileiras | 3,159 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 60.6 lb/ft³LPF/SFB Madeiras Brasileiras | 73.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 20,595 lb/in²LPF/SFB Madeiras Brasileiras | 22,871 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.38 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,275 lb/in²LPF/SFB Madeiras Brasileiras | 12,531 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.2%LPF/SFB Madeiras Brasileiras | 13.2%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.69LPF/SFB Madeiras Brasileiras | 1.86LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Pracuúba-da-terra-firme carries 11% more load in bending, which matters for a shelf or a rail.
- Pracuúba-da-terra-firme is the heavier of the two by 206 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.