Wood Record

Cachaporra-do-gentio vs Sapucaia

Terminalia cf argentea against Lecythis spp.. Every number below names the publication it came from.

PropertyCachaporra-do-gentioSapucaia
Janka hardness3,139 lbfLPF/SFB Madeiras Brasileiras3,100 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC60.6 lb/ft³LPF/SFB Madeiras Brasileiras58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture20,595 lb/in²LPF/SFB Madeiras Brasileiras27,540 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.38 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength12,275 lb/in²LPF/SFB Madeiras Brasileiras13,280 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)15.2%LPF/SFB Madeiras Brasileiras13.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.69LPF/SFB Madeiras Brasileiras1.27Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Sapucaia moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.7, so it is the safer choice for a wide flat panel.
  • Sapucaia carries 34% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons