Wood Record

Canafístula vs Oak

Cassia fastuosa against Quercus spp.. Every number below names the publication it came from.

PropertyCanafístulaOak
Janka hardness2,500 lbfLPF/SFB Madeiras Brasileiras2,500 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC54.3 lb/ft³LPF/SFB Madeiras Brasileiras53.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture16,527 lb/in²LPF/SFB Madeiras Brasileiras23,000 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.91 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.02 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength10,469 lb/in²LPF/SFB Madeiras Brasileiras2,960 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)—18.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.47LPF/SFB Madeiras Brasileiras1.83USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Canafístula moves more evenly. Its tangential-to-radial ratio is 1.5 against 1.8, so it is the safer choice for a wide flat panel.
  • Oak carries 39% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons