PropertyCanafístulaUrucurana
Janka hardness2,500 lbfLPF/SFB Madeiras Brasileiras2,469 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC54.3 lb/ft³LPF/SFB Madeiras Brasileiras57.4 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture16,527 lb/in²LPF/SFB Madeiras Brasileiras22,345 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.91 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.42 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength10,469 lb/in²LPF/SFB Madeiras Brasileiras10,596 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—15.0%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.47LPF/SFB Madeiras Brasileiras1.37LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Urucurana carries 35% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.