Caraipé vs Tanimbuca
Licania octandra against Buchenavia sp. Every number below names the publication it came from.
| Property | Caraipé | Tanimbuca |
|---|---|---|
| Janka hardness | 2,754 lbfLPF/SFB Madeiras Brasileiras | 2,829 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 61.3 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 53.7 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 23,355 lb/in²LPF/SFB Madeiras Brasileiras | 19,756 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.47 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.03 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,090 lb/in²LPF/SFB Madeiras Brasileiras | 10,582 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 17.4%LPF/SFB Madeiras Brasileiras | 12.7%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.95LPF/SFB Madeiras Brasileiras | 1.89LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 3%. Choose on movement or on appearance instead.
- Caraipé carries 18% more load in bending, which matters for a shelf or a rail.
- Caraipé is the heavier of the two by 122 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.