Caraiperana vs Castanha-de-cutia
Licania gracilipes against Couepia robusta. Every number below names the publication it came from.
| Property | Caraiperana | Castanha-de-cutia |
|---|---|---|
| Janka hardness | 3,294 lbfLPF/SFB Madeiras Brasileiras | 3,206 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 63.7 lb/ft³LPF/SFB Madeiras Brasileiras | 64.3 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 22,986 lb/in²LPF/SFB Madeiras Brasileiras | 22,416 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.35 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.26 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,247 lb/in²LPF/SFB Madeiras Brasileiras | 11,436 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 18.1%LPF/SFB Madeiras Brasileiras | 15.7%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 2.27LPF/SFB Madeiras Brasileiras | 1.90LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 3%. Choose on movement or on appearance instead.
- Castanha-de-cutia moves more evenly. Its tangential-to-radial ratio is 1.9 against 2.3, so it is the safer choice for a wide flat panel.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.