Maytenus spp. against Mora spp.. Every number below names the publication it came from.

PropertyCarne D'AntaMora
Janka hardness2,240 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,300 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC54.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture18,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)22,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.41 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.96 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength11,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,840 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)—18.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.93Chudnoff 1984, Tropical Timbers of the World (AH-607)1.42USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 3%. Choose on movement or on appearance instead.
  • Mora moves more evenly. Its tangential-to-radial ratio is 1.4 against 1.9, so it is the safer choice for a wide flat panel.
  • Mora carries 21% more load in bending, which matters for a shelf or a rail.
  • Mora is the heavier of the two by 128 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.