Casca-preciosa vs Muirapixuna

Aniba canelilla against Chamaecrista scleroxylon = Cassia scleroxylon. Every number below names the publication it came from.

PropertyCasca-preciosaMuirapixuna
Janka hardness3,369 lbfLPF/SFB Madeiras Brasileiras3,435 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC75.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-984.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture26,668 lb/in²LPF/SFB Madeiras Brasileiras26,227 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.55 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.38 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength14,180 lb/in²LPF/SFB Madeiras Brasileiras13,967 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.6%LPF/SFB Madeiras Brasileiras11.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.28LPF/SFB Madeiras Brasileiras2.28LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 2%. Choose on movement or on appearance instead.
  • Casca-preciosa moves more evenly. Its tangential-to-radial ratio is 1.3 against 2.3, so it is the safer choice for a wide flat panel.
  • Muirapixuna is the heavier of the two by 140 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.