Castanha-de-cutia vs Leche Perra
Acioa edulis against Helicostylis tomentosa. Every number below names the publication it came from.
| Property | Castanha-de-cutia | Leche Perra |
|---|---|---|
| Janka hardness | 2,696 lbfLPF/SFB Madeiras Brasileiras | 2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 64.9 lb/ft³LPF/SFB Madeiras Brasileiras | 55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 21,847 lb/in²LPF/SFB Madeiras Brasileiras | 22,800 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.36 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.86 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 11,748 lb/in²LPF/SFB Madeiras Brasileiras | 12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 17.5%LPF/SFB Madeiras Brasileiras | 14.6%Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Tangential / radial ratio(lower is better) | 1.28LPF/SFB Madeiras Brasileiras | 1.70Chudnoff 1984, Tropical Timbers of the World (AH-607) |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Castanha-de-cutia moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.7, so it is the safer choice for a wide flat panel.
- Castanha-de-cutia is the heavier of the two by 159 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.