Castanha-de-cutia vs Castanha-de-cutia
Couepia robusta against Acioa edulis. Every number below names the publication it came from.
| Property | Castanha-de-cutia | Castanha-de-cutia |
|---|---|---|
| Janka hardness | 3,206 lbfLPF/SFB Madeiras Brasileiras | 2,696 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 64.3 lb/ft³LPF/SFB Madeiras Brasileiras | 64.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 22,416 lb/in²LPF/SFB Madeiras Brasileiras | 21,847 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.26 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.36 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,436 lb/in²LPF/SFB Madeiras Brasileiras | 11,748 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.7%LPF/SFB Madeiras Brasileiras | 17.5%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.90LPF/SFB Madeiras Brasileiras | 1.28LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Castanha-de-cutia resists denting better. It tests 19% harder than Castanha-de-cutia.
- Castanha-de-cutia moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.9, so it is the safer choice for a wide flat panel.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.