Castanha-de-cutia vs Macucu-branco
Couepia robusta against Licania oblongifolia. Every number below names the publication it came from.
| Property | Castanha-de-cutia | Macucu-branco |
|---|---|---|
| Janka hardness | 3,206 lbfLPF/SFB Madeiras Brasileiras | 3,153 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 64.3 lb/ft³LPF/SFB Madeiras Brasileiras | 58.7 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 22,416 lb/in²LPF/SFB Madeiras Brasileiras | 19,429 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.26 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.19 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,436 lb/in²LPF/SFB Madeiras Brasileiras | 10,895 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.7%LPF/SFB Madeiras Brasileiras | 19.6%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.90LPF/SFB Madeiras Brasileiras | 1.97LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 2%. Choose on movement or on appearance instead.
- Castanha-de-cutia carries 15% more load in bending, which matters for a shelf or a rail.
- Castanha-de-cutia is the heavier of the two by 90 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.