Chengal vs Pyinkado
Balanocarpus spp. against Xylia xylocarpa. Every number below names the publication it came from.
| Property | Chengal | Pyinkado |
|---|---|---|
| Janka hardness | 2,130 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,248 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 61.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 21,560 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 21,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.84 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | — |
| Crushing strength | 10,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | — | 11.1%Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Tangential / radial ratio(lower is better) | — | 2.03Chudnoff 1984, Tropical Timbers of the World (AH-607) |
What the numbers mean
- Pyinkado resists denting better. It tests 6% harder than Chengal.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.