PropertyCourbarilFava-orelha-de-negro
Janka hardness2,350 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,346 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture19,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b23,440 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.16 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.43 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,510 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b11,407 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)12.7%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-412.7%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.89USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-42.21LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Courbaril moves more evenly. Its tangential-to-radial ratio is 1.9 against 2.2, so it is the safer choice for a wide flat panel.
  • Fava-orelha-de-negro carries 21% more load in bending, which matters for a shelf or a rail.
  • Fava-orelha-de-negro is the heavier of the two by 96 kg/m³, which a reader building a door or a case should weigh.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.