Courbaril vs Fustic
Hymenaea courbaril against Chlorophora tinctoria. Every number below names the publication it came from.
| Property | Courbaril | Fustic |
|---|---|---|
| Janka hardness | 2,350 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2,380 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 19,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 19,560 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.16 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2.16 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 9,510 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 11,080 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | 12.7%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 7.8%Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Tangential / radial ratio(lower is better) | 1.89USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 1.59Chudnoff 1984, Tropical Timbers of the World (AH-607) |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Fustic moves more evenly. Its tangential-to-radial ratio is 1.6 against 1.9, so it is the safer choice for a wide flat panel.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.