Cumaru vs Maria-preta
Dipteryx odorata against Zizyphus cinnamomum = Zizyphus itacaiunensis. Every number below names the publication it came from.
| Property | Cumaru | Maria-preta |
|---|---|---|
| Janka hardness | 3,415 lbfLPF/SFB Madeiras Brasileiras | 3,331 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 66.8 lb/ft³LPF/SFB Madeiras Brasileiras | 60.6 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 24,371 lb/in²LPF/SFB Madeiras Brasileiras | 22,714 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.43 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.35 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 14,742 lb/in²LPF/SFB Madeiras Brasileiras | 12,688 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 13.5%LPF/SFB Madeiras Brasileiras | 15.7%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.56LPF/SFB Madeiras Brasileiras | 1.43LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 3%. Choose on movement or on appearance instead.
- Cumaru is the heavier of the two by 100 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.