Demerara Greenheart vs Fava-orelha-de-negro

Ocotea rodiaei against Enterolobium schomburgkii. Every number below names the publication it came from.

PropertyDemerara GreenheartFava-orelha-de-negro
Janka hardness2,360 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,346 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)23,440 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity3.04 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.43 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength13,040 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,407 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)17.1%Chudnoff 1984, Tropical Timbers of the World (AH-607)12.7%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.09Chudnoff 1984, Tropical Timbers of the World (AH-607)2.21LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Demerara Greenheart moves more evenly. Its tangential-to-radial ratio is 1.1 against 2.2, so it is the safer choice for a wide flat panel.
  • Demerara Greenheart carries 12% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons