Wood Record

Demerara Greenheart vs Fustic

Ocotea rodiaei against Chlorophora tinctoria. Every number below names the publication it came from.

PropertyDemerara GreenheartFustic
Janka hardness2,360 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,380 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)19,560 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity3.04 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.16 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength13,040 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)11,080 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)17.1%Chudnoff 1984, Tropical Timbers of the World (AH-607)7.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.09Chudnoff 1984, Tropical Timbers of the World (AH-607)1.59Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Demerara Greenheart moves more evenly. Its tangential-to-radial ratio is 1.1 against 1.6, so it is the safer choice for a wide flat panel.
  • Demerara Greenheart carries 34% more load in bending, which matters for a shelf or a rail.
  • Demerara Greenheart is the heavier of the two by 160 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons