Demerara Greenheart vs Greenheart
Ocotea rodiaei against Chlorocardium rodiei. Every number below names the publication it came from.
| Property | Demerara Greenheart | Greenheart |
|---|---|---|
| Janka hardness | 2,360 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,350 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Density at 12% MC | 66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 24,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Modulus of elasticity | 3.04 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 3.25 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Crushing strength | 13,040 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 12,510 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b |
| Volumetric shrinkage(lower is better) | 17.1%Chudnoff 1984, Tropical Timbers of the World (AH-607) | 17.1%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 |
| Tangential / radial ratio(lower is better) | 1.09Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.09USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.