Demerara Greenheart vs Uxi
Ocotea rodiaei against Endopleura uchi. Every number below names the publication it came from.
| Property | Demerara Greenheart | Uxi |
|---|---|---|
| Janka hardness | 2,360 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,335 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 66.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 26,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 22,288 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.04 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 13,040 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 10,852 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 17.1%Chudnoff 1984, Tropical Timbers of the World (AH-607) | 15.6%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.09Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.50LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Demerara Greenheart moves more evenly. Its tangential-to-radial ratio is 1.1 against 1.5, so it is the safer choice for a wide flat panel.
- Demerara Greenheart carries 18% more load in bending, which matters for a shelf or a rail.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.