Wood Record

East African Olive vs Mecrusse

Olea hochstetteri against Androstachys johnsonii. Every number below names the publication it came from.

PropertyEast African OliveMecrusse
Janka hardness2,740 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,540 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture25,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)18,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.53 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Crushing strength12,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)—11.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—1.07Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • East African Olive resists denting better. It tests 8% harder than Mecrusse.
  • East African Olive carries 35% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons