Wood Record

East African Olive vs Missanda

Olea hochstetteri against Erythrophleum ivorense. Every number below names the publication it came from.

PropertyEast African OliveMissanda
Janka hardness2,740 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,930 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture25,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)23,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.53 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.24 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength12,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)14,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)——
Tangential / radial ratio(lower is better)——

What the numbers mean

  • Missanda resists denting better. It tests 7% harder than East African Olive.
  • East African Olive carries 8% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons