East Indian ebony vs Indian Laurel

Diospyros spp. against Terminalia tomentosa complex. Every number below names the publication it came from.

PropertyEast Indian ebonyIndian Laurel
Janka hardness1,630 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,220 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC52.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)54.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture11,125 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)15,380 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.44 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.91 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength5,960 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)8,275 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)14.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-413.2%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.63USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.54Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • Indian Laurel resists denting better. It tests 36% harder than East Indian ebony.
  • Indian Laurel carries 38% more load in bending, which matters for a shelf or a rail.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.