Fava-orelha-de-negro vs Greenheart

Enterolobium schomburgkii against Chlorocardium rodiei. Every number below names the publication it came from.

PropertyFava-orelha-de-negroGreenheart
Janka hardness2,346 lbfLPF/SFB Madeiras Brasileiras2,350 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture23,440 lb/in²LPF/SFB Madeiras Brasileiras24,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.43 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.25 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength11,407 lb/in²LPF/SFB Madeiras Brasileiras12,510 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)12.7%LPF/SFB Madeiras Brasileiras17.1%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)2.21LPF/SFB Madeiras Brasileiras1.09USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Greenheart moves more evenly. Its tangential-to-radial ratio is 1.1 against 2.2, so it is the safer choice for a wide flat panel.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.