Fava-orelha-de-negro vs Uxi

Enterolobium schomburgkii against Endopleura uchi. Every number below names the publication it came from.

PropertyFava-orelha-de-negroUxi
Janka hardness2,346 lbfLPF/SFB Madeiras Brasileiras2,335 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture23,440 lb/in²LPF/SFB Madeiras Brasileiras22,288 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.43 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,407 lb/in²LPF/SFB Madeiras Brasileiras10,852 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)12.7%LPF/SFB Madeiras Brasileiras15.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.21LPF/SFB Madeiras Brasileiras1.50LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Uxi moves more evenly. Its tangential-to-radial ratio is 1.5 against 2.2, so it is the safer choice for a wide flat panel.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.