Faveira-amargosa vs Faveira-amargosa
Vatairea paraensis against Vatairea guianensis. Every number below names the publication it came from.
| Property | Faveira-amargosa | Faveira-amargosa |
|---|---|---|
| Janka hardness | 2,174 lbfLPF/SFB Madeiras Brasileiras | 1,532 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 51.8 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 21,519 lb/in²LPF/SFB Madeiras Brasileiras | 16,059 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.18 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 1.93 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,280 lb/in²LPF/SFB Madeiras Brasileiras | 8,321 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 14.0%LPF/SFB Madeiras Brasileiras | 14.8%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 2.04LPF/SFB Madeiras Brasileiras | 2.03LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Faveira-amargosa resists denting better. It tests 42% harder than Faveira-amargosa.
- Faveira-amargosa carries 34% more load in bending, which matters for a shelf or a rail.
- Faveira-amargosa is the heavier of the two by 167 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.