Wood Record

Faveira-amargosa vs Mandioqueira

Vatairea paraensis against Qualea brevipedicellata. Every number below names the publication it came from.

PropertyFaveira-amargosaMandioqueira
Janka hardness2,174 lbfLPF/SFB Madeiras Brasileiras2,165 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-958.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture21,519 lb/in²LPF/SFB Madeiras Brasileiras19,145 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.18 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.26 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,280 lb/in²LPF/SFB Madeiras Brasileiras11,578 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)14.0%LPF/SFB Madeiras Brasileiras13.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.04LPF/SFB Madeiras Brasileiras1.95LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Faveira-amargosa carries 12% more load in bending, which matters for a shelf or a rail.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons