Faveira-amargosa vs Pau-amarelo

Vatairea paraensis against Euxylophora paraensis. Every number below names the publication it came from.

PropertyFaveira-amargosaPau-amarelo
Janka hardness2,174 lbfLPF/SFB Madeiras Brasileiras2,168 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-950.6 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture21,519 lb/in²LPF/SFB Madeiras Brasileiras17,566 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.18 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.92 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,280 lb/in²LPF/SFB Madeiras Brasileiras10,092 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)14.0%LPF/SFB Madeiras Brasileiras11.1%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.04LPF/SFB Madeiras Brasileiras1.36LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.
  • Pau-amarelo moves more evenly. Its tangential-to-radial ratio is 1.4 against 2.0, so it is the safer choice for a wide flat panel.
  • Faveira-amargosa carries 23% more load in bending, which matters for a shelf or a rail.
  • Faveira-amargosa is the heavier of the two by 187 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.