Wood Record

Fustic vs Matamatá

Chlorophora tinctoria against Eschweilera pedicellata = Eschweilera longipes. Every number below names the publication it came from.

PropertyFusticMatamatá
Janka hardness2,380 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,410 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)61.2 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture19,560 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)19,444 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.16 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.29 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,080 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,673 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)7.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)14.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.59Chudnoff 1984, Tropical Timbers of the World (AH-607)1.72LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Matamatá is the heavier of the two by 83 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons