Fustic vs Tuturubá
Chlorophora tinctoria against Pouteria gongrijpii = Franchetella gongrijpii. Every number below names the publication it came from.
| Property | Fustic | Tuturubá |
|---|---|---|
| Janka hardness | 2,380 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,396 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 56.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 19,560 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 20,951 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.16 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,080 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 10,952 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 7.8%Chudnoff 1984, Tropical Timbers of the World (AH-607) | 15.0%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.59Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.24LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Fustic moves more evenly. Its tangential-to-radial ratio is 1.6 against 2.2, so it is the safer choice for a wide flat panel.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.