Wood Record

Gangaw vs Indian rosewood

Mesua ferrea against Dalbergia latifolia. Every number below names the publication it came from.

PropertyGangawIndian rosewood
Janka hardness2,890 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)3,170 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC63.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)53.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture24,065 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)16,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity2.87 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.78 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength12,430 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,220 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)15.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)8.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.58Chudnoff 1984, Tropical Timbers of the World (AH-607)2.15USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • Indian rosewood resists denting better. It tests 10% harder than Gangaw.
  • Gangaw moves more evenly. Its tangential-to-radial ratio is 1.6 against 2.1, so it is the safer choice for a wide flat panel.
  • Gangaw carries 42% more load in bending, which matters for a shelf or a rail.
  • Gangaw is the heavier of the two by 160 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons