Wood Record

Goiabão vs Leche Perra

Chrysophyllum lucentifolium = Pouteria pachycarpa against Helicostylis tomentosa. Every number below names the publication it came from.

PropertyGoiabãoLeche Perra
Janka hardness2,646 lbfLPF/SFB Madeiras Brasileiras2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC58.1 lb/ft³LPF/SFB Madeiras Brasileiras55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture22,999 lb/in²LPF/SFB Madeiras Brasileiras22,800 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.41 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.86 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength11,357 lb/in²LPF/SFB Madeiras Brasileiras12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)16.5%LPF/SFB Madeiras Brasileiras14.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.81LPF/SFB Madeiras Brasileiras1.70Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 2%. Choose on movement or on appearance instead.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.