Indian Laurel vs Pyinkado

Terminalia tomentosa complex against Xylia xylocarpa. Every number below names the publication it came from.

PropertyIndian LaurelPyinkado
Janka hardness2,220 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,248 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC54.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)61.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture15,380 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)21,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.91 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Crushing strength8,275 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)13.2%Chudnoff 1984, Tropical Timbers of the World (AH-607)11.1%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.54Chudnoff 1984, Tropical Timbers of the World (AH-607)2.03Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Indian Laurel moves more evenly. Its tangential-to-radial ratio is 1.5 against 2.0, so it is the safer choice for a wide flat panel.
  • Pyinkado carries 38% more load in bending, which matters for a shelf or a rail.
  • Pyinkado is the heavier of the two by 112 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons