Ingá vs Sapucaia / sapucaia-vermelha
Inga sp against Lecythis pisonis subsp. usitata. Every number below names the publication it came from.
| Property | Ingá | Sapucaia / sapucaia-vermelha |
|---|---|---|
| Janka hardness | 2,846 lbfLPF/SFB Madeiras Brasileiras | 2,831 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 68.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 67.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 22,915 lb/in²LPF/SFB Madeiras Brasileiras | 21,747 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.25 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,905 lb/in²LPF/SFB Madeiras Brasileiras | 10,185 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 12.0%LPF/SFB Madeiras Brasileiras | 13.9%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 2.34LPF/SFB Madeiras Brasileiras | 1.43LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Sapucaia / sapucaia-vermelha moves more evenly. Its tangential-to-radial ratio is 1.4 against 2.3, so it is the safer choice for a wide flat panel.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.