Wood Record

Ipê vs Macawood

Handroanthus serratifolius = Tabebuia serratifolia against Platymiscium spp.. Every number below names the publication it came from.

PropertyIpêMacawood
Janka hardness3,100 lbfLPF/SFB Madeiras Brasileiras3,150 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC72.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-964.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture24,549 lb/in²LPF/SFB Madeiras Brasileiras27,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.86 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.20 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength12,360 lb/in²LPF/SFB Madeiras Brasileiras16,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)10.1%LPF/SFB Madeiras Brasileiras6.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.34LPF/SFB Madeiras Brasileiras1.30USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 2%. Choose on movement or on appearance instead.
  • Macawood carries 12% more load in bending, which matters for a shelf or a rail.
  • Ipê is the heavier of the two by 136 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons