Ipe vs Jataipeba
Tabebuia spp., lapacho group against Dialium guianense. Every number below names the publication it came from.
| Property | Ipe | Jataipeba |
|---|---|---|
| Janka hardness | 3,680 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 3,650 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 70.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 63.7 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 25,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 24,614 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.14 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2.35 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 13,010 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 12,481 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 13.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 14.5%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.21USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 1.75LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Ipe moves more evenly. Its tangential-to-radial ratio is 1.2 against 1.7, so it is the safer choice for a wide flat panel.
- Ipe is the heavier of the two by 101 kg/m³, which a reader building a door or a case should weigh.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.